The reason for the oxidation of the metal wire drawing of the wire drawing machine

1. The temperature of the cooling water in the sealing chamber of the metal wire drawing machine is too high, exceeding 40 °C, so that the sealing chamber cannot achieve the required cooling effect on the metal wire, resulting in the temperature of the single wire after annealing is still high, and the oxidized by oxygen in the air.

2. The saponified liquid content of the coolant in the sealing chamber is not enough, which will increase the friction between the wire and each guide wheel, and then the temperature of the wire will rise again, causing the surface of the wire to oxidize.

3. The water pressure and water volume of the cooling water in the sealed chamber are not enough, so that the metal wire cannot achieve a satisfactory cooling effect.